EXPERIMENTAL STUDY THE MECHANICAL PROPERTIES OF GMAW WELDING RESULTS ON S355J2+N MATERIAL WITH POST WELD HEAT TREATMENT (PWHT)
Assembly underframe trains are a connecting process part-part into a system that has a unified function, the process of which uses GMAW-type welding. From the welding results, there is potential for the formation of residual stress which is a problem in this research, so it is minimized using the me...
Saved in:
Main Authors: | , , , , |
---|---|
Format: | UMS Journal (OJS) |
Language: | eng |
Published: |
Universitas Muhammadiyah Surakarta
2024
|
Subjects: | |
Online Access: | https://journals2.ums.ac.id/index.php/mesin/article/view/2848 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
_version_ | 1805340886931865600 |
---|---|
author | Arif, Muhammad Yuwono, Indarto Salim, Alfi Tranggono Agus Dharmawan, Alit Zuriah, Dara Lathiful |
author_facet | Arif, Muhammad Yuwono, Indarto Salim, Alfi Tranggono Agus Dharmawan, Alit Zuriah, Dara Lathiful |
author_sort | Arif, Muhammad |
collection | OJS |
description | Assembly underframe trains are a connecting process part-part into a system that has a unified function, the process of which uses GMAW-type welding. From the welding results, there is potential for the formation of residual stress which is a problem in this research, so it is minimized using the method Post Weld Heat Treatment (PWHT) thermal. The research aims to determine and analyze the effect of PWHT on the mechanical properties and microstructure of low-carbon steel type S355J2+N resulting from GMAW welding. The research method uses experiments with PWHT temperatures at 450 °C, 750 °C, and non-PWHT to find out the mechanical properties of materials, use the tensile test and micro-Vickers hardness test. Meanwhile, to determine the microstructure formed is used micro examination. The test results, were compared between the welding material with PWHT and the welding material non-PWHT. The results of the research are that the largest tensile strength value of 576 MPa was produced in the material using PWHT at a temperature of 450 °C, the largest elongation of 34.85% was produced in the material with a PWHT temperature of 750 °C, and the highest hardness value was 207.44 HV in the material non-PWHT. The conclusion of the research shows that with increasing PWHT temperature, the hardness and tensile strength values of the material decrease, and there is an increase in the ductility value of the material which is influenced by changes in the dominance of ferrite and pearlite in the material. |
format | UMS Journal (OJS) |
id | oai:ojs2.journals2.ums.ac.id:article-2848 |
institution | Universitas Muhammadiyah Surakarta |
language | eng |
publishDate | 2024 |
publisher | Universitas Muhammadiyah Surakarta |
record_format | ojs |
spelling | oai:ojs2.journals2.ums.ac.id:article-2848 EXPERIMENTAL STUDY THE MECHANICAL PROPERTIES OF GMAW WELDING RESULTS ON S355J2+N MATERIAL WITH POST WELD HEAT TREATMENT (PWHT) Arif, Muhammad Yuwono, Indarto Salim, Alfi Tranggono Agus Dharmawan, Alit Zuriah, Dara Lathiful PWHT GMAW S355J2+N sifat mekanik struktur mikro Assembly underframe trains are a connecting process part-part into a system that has a unified function, the process of which uses GMAW-type welding. From the welding results, there is potential for the formation of residual stress which is a problem in this research, so it is minimized using the method Post Weld Heat Treatment (PWHT) thermal. The research aims to determine and analyze the effect of PWHT on the mechanical properties and microstructure of low-carbon steel type S355J2+N resulting from GMAW welding. The research method uses experiments with PWHT temperatures at 450 °C, 750 °C, and non-PWHT to find out the mechanical properties of materials, use the tensile test and micro-Vickers hardness test. Meanwhile, to determine the microstructure formed is used micro examination. The test results, were compared between the welding material with PWHT and the welding material non-PWHT. The results of the research are that the largest tensile strength value of 576 MPa was produced in the material using PWHT at a temperature of 450 °C, the largest elongation of 34.85% was produced in the material with a PWHT temperature of 750 °C, and the highest hardness value was 207.44 HV in the material non-PWHT. The conclusion of the research shows that with increasing PWHT temperature, the hardness and tensile strength values of the material decrease, and there is an increase in the ductility value of the material which is influenced by changes in the dominance of ferrite and pearlite in the material. Universitas Muhammadiyah Surakarta 2024-01-30 info:eu-repo/semantics/article info:eu-repo/semantics/publishedVersion Peer-reviewed Article application/pdf https://journals2.ums.ac.id/index.php/mesin/article/view/2848 Media Mesin: Majalah Teknik Mesin; Vol. 25 No. 1 (2024); 1-9 2541-4577 1411-4348 eng https://journals2.ums.ac.id/index.php/mesin/article/view/2848/1059 Copyright (c) 2024 Muhammad Arif, Indarto Yuwono, Alfi Tranggono Agus Salim, Alit Dharmawan, Dara Lathiful Zuriah https://creativecommons.org/licenses/by/4.0 |
spellingShingle | PWHT GMAW S355J2+N sifat mekanik struktur mikro Arif, Muhammad Yuwono, Indarto Salim, Alfi Tranggono Agus Dharmawan, Alit Zuriah, Dara Lathiful EXPERIMENTAL STUDY THE MECHANICAL PROPERTIES OF GMAW WELDING RESULTS ON S355J2+N MATERIAL WITH POST WELD HEAT TREATMENT (PWHT) |
title | EXPERIMENTAL STUDY THE MECHANICAL PROPERTIES OF GMAW WELDING RESULTS ON S355J2+N MATERIAL WITH POST WELD HEAT TREATMENT (PWHT) |
title_full | EXPERIMENTAL STUDY THE MECHANICAL PROPERTIES OF GMAW WELDING RESULTS ON S355J2+N MATERIAL WITH POST WELD HEAT TREATMENT (PWHT) |
title_fullStr | EXPERIMENTAL STUDY THE MECHANICAL PROPERTIES OF GMAW WELDING RESULTS ON S355J2+N MATERIAL WITH POST WELD HEAT TREATMENT (PWHT) |
title_full_unstemmed | EXPERIMENTAL STUDY THE MECHANICAL PROPERTIES OF GMAW WELDING RESULTS ON S355J2+N MATERIAL WITH POST WELD HEAT TREATMENT (PWHT) |
title_short | EXPERIMENTAL STUDY THE MECHANICAL PROPERTIES OF GMAW WELDING RESULTS ON S355J2+N MATERIAL WITH POST WELD HEAT TREATMENT (PWHT) |
title_sort | experimental study the mechanical properties of gmaw welding results on s355j2 n material with post weld heat treatment pwht |
topic | PWHT GMAW S355J2+N sifat mekanik struktur mikro |
topic_facet | PWHT GMAW S355J2+N sifat mekanik struktur mikro |
url | https://journals2.ums.ac.id/index.php/mesin/article/view/2848 |
work_keys_str_mv | AT arifmuhammad experimentalstudythemechanicalpropertiesofgmawweldingresultsons355j2nmaterialwithpostweldheattreatmentpwht AT yuwonoindarto experimentalstudythemechanicalpropertiesofgmawweldingresultsons355j2nmaterialwithpostweldheattreatmentpwht AT salimalfitranggonoagus experimentalstudythemechanicalpropertiesofgmawweldingresultsons355j2nmaterialwithpostweldheattreatmentpwht AT dharmawanalit experimentalstudythemechanicalpropertiesofgmawweldingresultsons355j2nmaterialwithpostweldheattreatmentpwht AT zuriahdaralathiful experimentalstudythemechanicalpropertiesofgmawweldingresultsons355j2nmaterialwithpostweldheattreatmentpwht |